论文部分内容阅读
我厂的MQG φ3200/3100湿式格子型球磨机,在 1999年12月底检修时发现大、小V形衬板磨损 严重,造成出料端盖肋板及轴颈内侧不同程度地磨 损,经有关 技术人员共 同研究决定 更换大、小 V形衬板, 按原设计要 求,大、小V 形衬板与出 料端盖之间 隙需要8
I plant MQG φ3200 / 3100 wet lattice ball mill, at the end of December 1999 overhaul found that large and small V-shaped liner wear and tear, resulting in the discharge end of the ribs and the journal neck wear to varying degrees, the relevant technical staff Joint research decided to replace the large and small V-shaped liner, according to the original design requirements, large and small V-shaped liner and the gap required for the material cover 8