论文部分内容阅读
1种乙烯-四氟乙烯共聚物浆液的后处理方法,它包括如下步骤:1)提供乙烯-四氟乙烯共聚物浆液;2)过滤后以0.2~2L/kg滤饼的量向滤饼中加入水,在10~110℃的温度下以10~300 r/min的速度搅拌1~120 min;3)干燥后形成乙烯-四氟乙烯共聚物颗粒。(CN103497270A)
1) ethylene-tetrafluoroethylene copolymer slurry after-treatment method, comprising the steps of: 1) providing an ethylene-tetrafluoroethylene copolymer slurry; 2) After filtering the amount of 0.2 ~ 2L / kg filter cake into the filter cake Adding water, stirring at a speed of 10 to 300 r / min for 1 to 120 minutes at a temperature of 10 to 110 DEG C; and 3) drying to form ethylene-tetrafluoroethylene copolymer particles. (CN103497270A)