In order to improve the filling ability of large complex thin wall castings, the pouring temperature should be increased, but this will result in the grain coar
Ti6Al4V substrates were anodized in a 0.5 mol/L H_2SO_4 solution at applied voltages of 90-140 V.A hydroxyapatite-titanium oxide(HA-TiO2)coating was then deposi