论文部分内容阅读
砖坯的自然干燥是一道极为重要的工序。天津地区的砖瓦企业总結了这方面的經驗,現扼要介紹如下。一、平修架埂。为了保証砖坯上架后不走形变样,架底坯子不裂,須平修好碼放砖坯的架埂。架埂寬度不得少于80厘米,高度要比地面高出25—30厘米,长度可根据場地条件适当确定?艿理毐3忠欢ǖ钠露?以便雨水排出,防止因泄水緩慢而造成倒架事故。平修架埂时翻掘土的深度不能浅于2寸。地势低洼,
The natural drying of bricks is an extremely important process. The brick and tile enterprises in the Tianjin region have summarized the experience in this area and are now briefly introduced below. First, the frame of repair. In order to ensure that the bricks do not go out of shape after the shelf, the bottom billet does not crack, you must repair the stacking of bricks. The width of the frame must not be less than 80 centimeters, and the height should be 25-30 centimeters higher than the ground. The length can be properly determined according to the site conditions. The solution can be used to prevent the water from being discharged due to the slow discharge of water. Accidents. The depth of digging soil when the frame is leveled is not to be less than 2 inches. Low-lying,