Both Mg-1Mn-3.5Y and Mg-1Mn-1Y-2.5Nd alloys (mass fraction, %) were extruded at 380 ℃. Most of the (10(1)0) crystal planes in the Mg-1Mn-3.5Y alloy are paralle
AZ80 magnesium alloys were deformed at 200, 250, 300, 350 and 400 ℃ with different deformation degree of 50%, 75%, 83%, 87% and 90%, respectively. The corrosio