Si-Ti-B掺杂金刚石/硬质合金复合体的性能

来源 :北京科技大学学报 | 被引量 : 0次 | 上传用户:liedh123
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
金刚石粒度和掺杂量两因素对Si-Ti-B掺杂金刚石/硬质合金复合体的金刚石层的抗弯强度和耐磨性的综合影响,可以归结为平均自由程与机械性能的关系。在强度(或耐磨性)与平均自由程的关系曲线中,存在最大值。对于低掺杂量材料,强度随平均自由程(粘结相层厚度)的减少而降低。对于高掺杂量材料,强度随粘结相层厚度的增大而下降。Si-Ti-B掺杂烧结金刚石的耐热性高于钴粘结金刚石。 The combined effect of diamond particle size and doping amount on the flexural strength and wear resistance of the diamond layer of Si-Ti-B-doped diamond / cemented carbide composites can be attributed to the relationship between mean free path and mechanical properties. In the relationship between strength (or wear resistance) and mean free path, there is a maximum value. For low doping materials, the strength decreases with decreasing mean free path (thickness of binder phase). For high doping materials, the strength decreases with the increase of the thickness of the binder phase. The heat resistance of Si-Ti-B doped sintered diamond is higher than that of cobalt bonded diamond.
其他文献
炭材料具有重量轻、耐热性等其它材料所不具备的特性。因此在许多领域作为工业材料使用。最近正在开发新的制造方法,控制产品的物性及具有新结构和功能的材料,也在开发新的用
本文利用透射电子显微镜、X光、化学物相分析等研究和证实了方铅矿中次显微金的赋存状态,从而为金的选矿方法、流程设计及金的回收工艺提供了重要的依据。 In this paper, t
为开发毫米波吸波体,测量了碳化硅纤维增强塑料在毫米波段(50GHz)的吸波特性。结果显示,在频率为57~58GHz时最大吸收量为17~20dB左右。实验证明,通过严格控制塑料薄膜厚度和正
日本日立金属有限公司称已研制出一种具有高温高强度的低价燃气涡轮盘锻造合金SDA—2。目的在于取代目前强度最高的粉末冶金燃气涡轮盘合金。 这种镍基锻造合金的成分中除了
内容简介:自幼憧憬惊吓专员职业的大眼仔麦克·华斯基,终于如愿考入曾走出过无数传奇人物的怪兽大学惊吓学院。对于这个相貌讨喜、丝毫没有任何恐怖气场的小怪物来说,死啃书
称作“白石墨”六方晶 BN(h-BN),不仅具有石墨相类似的层状结构、机械切削加工性、润滑性、耐热性、耐热冲击性、耐侵蚀性等方面的优越性能,而且也具有与导电性石墨不同的电
本文研究了Ni_3Al基合金的元素组成、组织控制及其与力学性能之间的关系。探索表明:B、Al、Mo是影响Ni_3Al基高温合金组织与性能的三种主要元素;γ’单相区的尺寸和数量对合
本文用DTA和X射线衍射技术,研究了(FeCr)_(83)B_(17)非晶合金晶化相变全过程。说明该非晶体系的晶化相变过程中,原子键力是晶化相变的驱动力。从“t-x”关系表明,在我们实验
采用B_2O_3玻璃和纯循环过热净化相结合的方法去除液态金属中的异质晶核,使液态Ni-7.3%Si-2.2%B合金获得了330K的过冷度。对比分析了该合金在低温基板上的快淬薄片与大体积深过
由西安工业学院材料工程系承担的《Fe-Al金属间化合物的韧化研究》课题,于1993年3月22日在西安通过了由兵器科学研究院主持的技术鉴定。鉴定委员会认为,该项研究采用稀土等