Through the experiment, the reduced temperature, the containing scandium quantity of the fused salt, the agitated intensity and the restoring time that influenc
Microstructure and magnetic properties of Nd8.5Fe77.1B6.4Co4Zr3Nb0.5V0.5 nanocomposite ribbons were investigated. A fine and uniform grain with 30 nm in average