为了评价聚变堆包层用Fe-Al/Al_2O_3复合涂层的阻氚性能,建立系统、准确的涂层材料中氢同位素浓度深度分布的分析方法,选择了CLAM钢基材、Fe_2Al_5渗铝层、Fe-Al/Al_2O_3、Fe-Al/α-Al_2O_3复合涂层等典型样品作为研究对象,开展了模拟聚变堆产氚包层(TBM)工况下(550℃温度、1 kPa氘/氚压条件)的充氘及渗氚实验,采用辉光放电光谱(GDOES)、氚成像(TIP)及氚β衰变韧 In order to evaluate the resistance and trituration performance of the Fe-Al / Al_2O_3 composite coating for fusion cladding, a systematic and accurate analytical method for the depth distribution of hydrogen isotopes in the coating materials was established. The CLAM steel substrate, Fe_2Al_5 aluminized layer, Fe-Al / Al_2O_3 and Fe-Al / α-Al_2O_3 composite coatings were selected as the research objects. Under the conditions of 550 ℃ and 1 kPa deuterium / tritium pressure ) Deuterium infiltration and trituration experiments, using glow discharge spectroscopy (GDOES), tritium imaging (TIP) and tritium beta decay toughness
其他文献
新兴大国在赶超发展中普遍面临着后劲不足的挑战。培育新的增长源头成为其摆脱困境的不二选择。而发展新兴产业是新兴经济体调整产业结构,加快增长方式转变、保持赶超发展态
聚变堆氚工厂氚分析与检测技术是实现聚变堆氘氚燃料循环系统燃料及工艺气体组分含量的检测分析,以确保聚变堆的安全稳定运行,并监控氚向环境的排放,以保障公众辐射防护安全
腔耦合直线加速器(CCL)是大型质子直线加速器关键的常温加速结构,在国外获得了深入的研究与应用。本文对CCL进行了电磁场的设计与模拟计算和多能量加速的研究。腔体的机械尺
离子源是强流质子加速器的关键部件,国内外对其进行了大量深入的研究与应用工作。本文对离子源的选型与方案设计进行了相关工作。首先调研质子源和负氢离子源的工作原理、设
轻水堆核电站燃料棒一旦发生破损,燃料中的放射性裂变产物就会释放到一回路的冷却剂中,会给核电站的安全性和经济性造成不良影响。所以燃料包壳的破损问题是国际上一个重要的
为了对电磁同位素分离器离子源的束流性能进行测试,研制了3套检测设备,即张角测量仪、发射度仪和谱线扫描装置,用于电磁分离器的调试和优化。张角测量仪用于测量离子源引出束
CAP1400大型先进压水堆示范工程是我国在AP1000核电技术上进行再创新而建成的。在其设计中,对于国产主管道材料能否用RG1.207导则进行疲劳寿命曲线的修订是其设计的一个难题,
2014年,稳定同位素电磁分离中心对同位素电磁分离器进行综合技术改造,其中的一个创新点就是将计算机控制技术与同位素电磁分离器相结合,同位素电磁分离器计算机控制系统是通
稳定同位素电磁分离中心于2013年开展了F-3电磁分离器综合技术改造项目,保留原有的180°电磁铁及真空室,同时引进新型科技,以提高电磁分离器的分离效率,并实现了自动化控制。
串列升级工程需要建造6条质子束流输运线来将100 MeV回旋加速引出的强流质子束传输到生产和实验终端。其中从北向引出口引出的一条向正北方向传输束流线将质子束流传输至同位