【摘 要】
:
The nickel-iron metal supported solid oxide fuel cells fabricated by atmospheric plasma spraying(APS)are heat treated in air at 850℃ for 4 hours.The electrolytes of these cells are produced by differe
【机 构】
:
Physics Division,Institute of Nuclear Energy Research,Lungtan,Taoyuan 32546,Taiwan,ROC
论文部分内容阅读
The nickel-iron metal supported solid oxide fuel cells fabricated by atmospheric plasma spraying(APS)are heat treated in air at 850℃ for 4 hours.The electrolytes of these cells are produced by different APS torch powers and other components of these cells are kept the same fabrication parameters.The XRD data of the prepared cells show that there are no impurity phases except the 54 kW samples in which the impurities caused by too high APS torch power exist.The current-voltage-power and AC impedance measurements show the prepared LSGM electrolyte using 52 kW APS torch power has a better electrochemical performance at temperatures ranging from 600 to 800oC.The different APS torch powers produce different electrolyte resistances during the cell fabrication and the prepared cell with 52 kW APS torch power has the lower electrolyte resistance at temperatures ranging from 600 to 800℃.
其他文献
在本研究中,我們探討(Ca0.95Sr0.05)(Ti1-xSnx)O3(x=0.01~0.09)之微波特性,由實驗得知(Ca0.95Sr0.05)(Ti0.97Sn0.03)O3 在燒結溫度1350℃持溫四小時擁有最佳微波介電特性:εr~91.23、Q × f~5242GHz、τf~+807.71 ppm/℃.為了跟(Ca0.8Sr0.2)TiO3(τf~+991 ppm/℃)有所區別,A-si
本實驗採用氧化物混合法(mixed oxide method)製作Mn0.1Mg0.9Fe2O4 陶瓷粉末,研究不同燒結溫度對微結構、晶格結構與交流磁化率的影響.鎂錳鐵氧化物經高溫燒結後XRD 結果顯示立方結構尖晶石,晶格常數會隨著燒結溫度提升而縮小.由OM 的表面觀察可以看到隨著燒接溫度的增加晶粒會隨著增加,且具有磁域結構.軟磁材料鎂錳鐵氧化物在交流頻率下磁化率的變化則呈現尼爾鬆弛行為,且燒結溫
The microstructures and dielectric properties of Zn2SnO4 thin films were investigated.Zn2SnO4 thin films were prepared using the radio frequency magnetron sputtering with various Ar/(Ar+O2)ratios.The
本研究採用水熱法藉由不同保護劑合成CuGaO2,探討在不同條件下對CuGaO2 粉末特性的影響,並分析其相成分、顯微結構及價態。本文藉由十六烷基三甲基氯化銨(Cetyltrimethylammonium chloride,CTAC)、十六烷基三甲基溴化銨(Cetyltrimethylammonium bromide,CTAB)作為保護劑以製備六角片狀之CuGaO2 粉末。此外,本實驗藉由氨水、去離
在固態氧化物燃料電池(SOFC)中,具磷灰石結構之矽酸鑭基電解質La9.8Si5.7Mg0.3O26.4(LSMO)擁有優良的導電率.本研究利用 Sr2+取代 LSMO 中部分 La3+,以固態合成法配製成 La9.8-xSrxSi5.7Mg0.3O26±δ(x = 0.2、0.4、0.6)系列之電解質,探討摻雜對矽酸鑭基固態電解質之微結構與導電率之影響.由研究結果發現,摻雜 Sr2+元素後造成燒
本研究採用常溫噴塗製程製作遠紅外線散熱膜,並探討遠紅外線材料配比及製程條件對LED 散熱基板之散熱效率的影響。常溫噴塗製程製作散熱膜是採用前人研發的遠紅外線粉末,添加有機溶劑製為塗料,在常溫的環境中以噴塗方式製成遠紅外線散熱膜,並探討遠紅外線粉末(1)不同黏結劑、(2)不同基板材質、(3)基板厚度、(4)有無噴塗,對LED 散熱的影響。最後在相同面積的純氧化鋁基板(直徑150×厚度2 ㎜)裝上1顆
本研究是以固態反應法製備中溫型固態氧化物燃料電池之Ce0.8Sm0.15 Ca0.05-xRxO2-δ(R= 0、0.025)電解質,選用在中溫(600~800 ℃)範圍下離子導電性較佳的CeO2 為基材,Ce0.8Sm0.2O2-δ(SDC)藉由共同摻雜Ca2+或Sr2+來改善電解質試片的緻密性,並且降低氧化铈基電解質的燒結溫度.電解質粉末以單軸加壓成型的方式製備出直徑為10 mm的圓盤碇,並控
本研究以固態反應法製備電解質Ce0.8Sm0.15Ca0.05O2–δ(SCDC)與La0.85Sr0.15Ga0.8Mg0.2O2.825(LSGM),以及陰極La0.6Sr0.4Co0.2Fe0.8O2–δ(LSCF6428),並混合陰極LSCF6428 與電解質SCDC 形成混合離子和電子導體(Mixed ionic andelectronic conductors,MIEC)之複合陰極9L
本研究成功利用溶膠凝膠法製備CeO2 基之電解質材料,藉由摻雜Sm、Ca、La、Sr 離子,製備Ce0.8Sm0.15R0.05O2-δ(R = Sm、Ca、La)及Ce0.8Sm0.15Ca0.025Sr0.025O2-δ 粉末,藉由產生氧缺陷來進行氧離子傳遞,並幫助晶粒成長.燒結溫度為1300 ℃ 並分別持溫2 小時與4 小時,與傳統固態合成法製備的粉末相比燒結溫度大幅降低,利用XRD、拉曼光
鋇鍶鈷鐵氧化物(Ba0.5Sr0.5Co0.8Fe0.2O3-(□□□□)BSCF))為具備混合離子-電子傳導之陶瓷氧化物,且具備高氧傳導率之特性.在本文中,BSCF 粉體由甘胺酸-硝酸鹽法(GNC)製備,並利用XRD 與ICP 量測粉體性質與成分組成.藉由刮刀成型技術及燒結程序製備BSCF 氧傳輸薄膜,並利用XRD 與SEM 分析其特性.根據XRD 與SEM 結果,BSCF 氧離子傳輸膜具單一鈣