论文部分内容阅读
Static and dynamic split tensile tests were conducted on rubber concrete with varied volume fractions of rubber particles that replaced fine aggregate(10%,20%,30%,40%,and 50%,named as RC10,RC20,RC30,RC40,and RC50,respectively).