论文部分内容阅读
Mullite-bonded porous silicon carbide(SiC)ceramics containing 30wt%nano-sized Al2O3 particles were prepared from four different SiC powders in air at 1450℃ for 3h.The surface of SiC particles was oxidized to SiO2,with further increasing the temperature,oxidation-derived SiO2 reacted with Al2O3 to form mullite,SiC particles were bonded by the mullite and oxidation-derived SiO2.