Ba0.85Ca0.15Ti0.9Zr0.1O3–xIr4+(BCZT–xIr,x=0–1.0%)ceramics were synthesized with as-prepared nanoparticles,which used by modified Pechini polymeric precursor method,sintered at low sintering temperature of 1260 ℃.